登录 查看组织和合同定价。
选择尺寸
变更视图
关于此项目
线性分子式:
I(CH2)8I
化学文摘社编号:
分子量:
366.02
UNSPSC Code:
12352100
NACRES:
NA.22
PubChem Substance ID:
EC Number:
246-456-6
Beilstein/REAXYS Number:
1735437
MDL number:
Assay:
98%
Form:
liquid
Quality Level
assay
98%
form
liquid
contains
copper as stabilizer
refractive index
n20/D 1.5653 (lit.)
bp
167-169 °C/6 mmHg (lit.)
density
1.84 g/mL at 25 °C (lit.)
functional group
iodo
SMILES string
ICCCCCCCCI
InChI
1S/C8H16I2/c9-7-5-3-1-2-4-6-8-10/h1-8H2
InChI key
KZDTZHQLABJVLE-UHFFFAOYSA-N
Application
1,8-二碘辛烷已用作加工添加剂以:
- 基于区域规整聚 3-己基噻吩和可溶性富勒烯衍生物改善体异质结太阳能电池的形貌和效率
- 提高聚合物太阳能电池的能量转换效率
hcodes
pcodes
Hazard Classifications
Aquatic Chronic 4
存储类别
10 - Combustible liquids
wgk
WGK 3
flash_point_f
235.4 °F - closed cup
flash_point_c
113 °C - closed cup
ppe
Eyeshields, Gloves, type ABEK (EN14387) respirator filter
Xing Fan et al.
Journal of nanoscience and nanotechnology, 14(5), 3592-3596 (2014-04-17)
Controlling the blend morphology is critical for achieving high power conversion efficiency in polymer/fullerene bulk heterojunction (BHJ) photovoltaic devices. As a simple and effective method to control morphology, adding processing additives has been widely applied in the organic BHJ solar
Satvik Shah et al.
Nanoscale, 9(25), 8665-8673 (2017-06-15)
Degradation is among the most pressing problems facing organic materials, occurring through ingress of moisture and oxygen, and light exposure. We determine the nanoscale pathways underlying degradation by light-soaking organic films in an environmental chamber, and performing infrared spectroscopy, to
Ali Aghassi et al.
Physical chemistry chemical physics : PCCP, 21(24), 13176-13185 (2019-06-08)
Contamination of the active layer with an impurity could result in significant degradation in the performance of bulk heterojunction (BHJ) solar cells as a result of enhancing the loss of the charge carriers via a trap-assisted recombination. In this study
全球贸易项目编号
| 货号 | GTIN |
|---|---|