grade
analytical standard
Quality Level
autoignition temp.
580 °F
shelf life
limited shelf life, expiry date on the label
mol wt
Mn ~1730, Mp ~1960, Mw ~1900
technique(s)
gel permeation chromatography (GPC): suitable
solubility
H2O: insoluble
density
1.200 g/cm3
Mw/Mn
~1.10
format
neat
storage temp.
2-8°C
InChI
1S/C5H9O2/c1-4(2)5(6)7-3/h1-3H3
InChI key
PMAMJWJDBDSDHV-UHFFFAOYSA-N
General description
聚甲基丙烯酸甲酯是一种刚性透明类型的高分子材料,通过甲基丙烯酸甲酯单体聚合获得。
Still not finding the right product?
Explore all of our products under 聚甲基丙烯酸甲酯
存储类别
11 - Combustible Solids
wgk
nwg
ppe
Eyeshields, Gloves, type N95 (US)
Biomechanics and Biomaterials in Orthopedics (2004)
Plastics Materials (1999)
Gursukhman S Sidhu et al.
Journal of neurosurgery. Spine, 19(1), 61-70 (2013-05-07)
The authors endeavor to highlight the surgical management of severe neurological deficit resulting from cement leakage after percutaneous vertebroplasty and to systematically review the literature on the management of this complication. A patient presented after a vertebroplasty procedure for traumatic
全球贸易项目编号
| 货号 | GTIN |
|---|---|
| 81489-500MG | 04061832879536 |